Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel

 

Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic

Key Words: EURONORM 1.4311 X2CrNiN18.10, AFNOR Z3CN 18.10Az, DIN W 1.4311, ASTM A240 TP 304LN, UNS S30453

Material Notes:
Description: CLC 18.10LN is a 18Cr-10Ni austenitic stainless steel with specific Nitrogen additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water quenching. Alloys CLC 18.10LN exhibits an austenitic microstructure free of deleterious carbide precipitations at grainboundaries. The grade contains some residual ferrite (=2%) after solution annealing (1050 - 1150°C / 1922 - 2102 °F) and water quenching. Nitrogen alloying :

  • improves tensile properties at room and moderate temperatures
  • improves structure stability of austenite at very low temperature or under severe cold deformations
  • does not affect weldability or fabricability
  • improves localized corrosion resistant properties
Typical applications are food processing industry, chemical industry.

Iron content calculated as remainder. Tensile properties after water quenching.

Information provided by manufacturer.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Creep Strength
  • Modulus of Elasticity
  • Poissons Ratio
  • Charpy Impact
  • Charpy Impact, Notched Low Temp
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。