MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel

 

Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Duplex

Key Words: EURONORM 1.4462 - X2 Cr Ni Mo N 22.5.3, AFNOR Z3 CND 22.05.AZ, WERKSTOFF Nr 1.4462, UNS S31803, UNS S32205

Material Notes:
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chromium. This alloy presents higher mechanical and corrosion resistance properties than duplex 22 Cr stainless steels. Its yield strength is about twice that of standard austenitic grades and well in excess of that of nitrogen alloyed austenitics. Operation temperature of UR 45 N+ is generally limited from -50°C to 280°C (- 58°F to 536°F). Lower temperature used particularly for welded structures may also be considered, but needs technical background.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Charpy Impact
  • Charpy Impact, Notched Low Temp
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。