Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment)

 

Subcategory: Stainless Steel; T S40000 Series Stainless Steel; Metal; Martensitic

Key Words: EURONORM 1.4006 X12 Cr 13, AFNOR Z 12 C 13, DIN W 1.4006 (DIN 17440), ASTM A240 TP 410, UNS S41000

Material Notes:
Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The grade has a martensitic microstructure. The final mechanical properties may be optimized by selecting an appropriate heat treatment. In the annealed conditions the alloy presents ductility and may be formed. Chromium additions (~13%) improve the corrosion resistance, particularly in wet conditions when compared to C-Mn steels. Slightly acidified and abrasion conditions are considered. The main applications concern mechanical industry, oil and gas industry, sugar industry and constructional components.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Charpy Impact
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。