Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel

 

Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic

Key Words: EN 10095 X9 Cr Ni Si N Ce 21-11-2 -1.4835, AFNOR (Z10 CNS 21 11), DIN W.Nr 1.4835, UNS S30815

Material Notes:
Description: CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthane,...etc) which make the alloy particularly well designed for high temperature applications. The nitrogen additions stabilize the austenitic microstructure, particularly at high temperatures. The alloy is less susceptible to embrittlements effects occurring after long term exposure. Creep properties are enhanced, due to high Chromium and Nitrogen. Rare Earth elements (Ce, La,...) are added in order to anchor the oxide protective film and improve the resistance of the steel to oxide spaling. As a result, the alloy is much more resistant to high temperature thermal cycling effects in oxidizing atmospheres compared to 310. CLI SIRIUS S15 grade may be used up to 1100°C (2012°F in oxidizing environments. Thermal cycling effects, sulphur containing atmospheres and low oxygen contents reduce the high temperature resistance of the steel.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Creep Strength
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。