Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel

 

Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal

Key Words: aisi304, aisi 304, DIN W.14306 Bor-01 Ind.00, ASTM A887 UNS S30464 : Type 304B4, SUS304, SS304

Material Notes:
Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL 18.10 B4 grade is a 304 stainless steel obtained by ingot casting and alloyed with 1 to 1,24 wt% natural boron additions. In order to avoid ferrite grain which reduce the ductility of the alloy, NUCL 18.10 B4 grade has been overalloyed in Nickel when compared to 304 grades. Molybdenum additions are sometimes considered to increase the corrosion resistance properties. The ingots rolled into plates are considered for nuclear applications (transport, casks, storage -in pools) of nuclear (waste) products. For specific purposes, some other grades are sometimes used. The boron content may thus be included in the 0.2-2 weight % range or/and alloys obtained by powder metallurgy (A type). CLI-FAFER can also produce 18-10 A or B type boron alloyed grades (included B10 enriched grades). Among the family of boron enriched 304 grades, NUCL 18-10 B4 grade is the most commonly used.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。