Industeel URANUS® B6N Multipurpose Austenitic Stainless Steel with PREN = 36

 

Subcategory: Stainless Steel; T 600 Series Stainless Steel; Metal; Austenitic

Key Words: EN 10088 - EN 10028.7 X1 Ni Cr Mo Cu 25.20.5 - 1.4539, AFNOR Z2 NCDU 25.20 (AZ), DIN W. Nr 1.4539, ASTM B 625 - UNS N08904

Material Notes:
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) to increase its structure stability and corrosion resistance. Due to combined additions of chromium (20%), molybdenum (4.3%), copper (1.5%) combined with its high nickel content, the grade is recommended for most applications dealing with medium to severe corrosive solutions. UR B6 has improved stress corrosion resistance properties. UR B6 alloy is particularly used in sulphuric and phosphoric acids applications. The localized corrosion resistance of UR B6N grade is much higher than that of alloy 825. UR B6N is particularly well adapted to clad plates applications (separators).

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Charpy Impact, Notched Low Temp
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。