Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel

 

Subcategory: Stainless Steel; Metal; Austenitic

Key Words: EURONORM X1 Ni Cr Mo Cu 31.27.4, AFNOR Z2 NCDU 31.27.03, DIN W. Nr 1.4563, UNS N08028

Material Notes:
Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for specific purposes, including sulphuric or phosphoric acid applications. It behaves particularly well in sulphuric and phosphoric acid environments, even when contaminated by chlorides and fluorides species. The high nickel content improves its stress corrosion cracking resistance. The combined chromium and molybdenum additions contribute to increase drastically the localized corrosion resistance. The alloy behaves much better than alloy 825 and could be considered in some applications (sour gas) to replace the more expensive 625 grade. The alloy is extensively used in chemical and offshore applications including very sour gas fields.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Charpy Impact, Notched Low Temp
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。