Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability

 

Subcategory: Carbon Steel; High Carbon Steel; Mold Steel; Metal

Key Words: AFNOR 40CMD8S, DIN 40CrMnMoS 8.6, WERKSTOFF Nbr 1.2312, AISI P20+S

Material Notes:
Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. The grade has a fully homogeneous martensite-bainite microstructure. CLC 1.2312 grade has specific sulfur addition (0.060% typical) in order to increase stronghtly it's machinability. Compared to CLC 1.2311 grade 30% increase in milling speed and 300% increase in drilling speed can be expected. At constant cutting speed, tool life is multiplied by a least 5 when replacing CLC 1.2311 by CLC1.2312 grade.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Charpy Impact
  • Charpy Impact, Notched Low Temp
  • Charpy Impact, Unnotched
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。