Industeel TENASTEEL® Cold Work Tool Steel

 

Subcategory: Tool Steel; Carbon Steel; High Carbon Steel; Metal

Material Notes:
Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and a particularly high resistance to thermal softening. The steel is delivered in the soft annealed condition with a maximum hardness of 250 HB. TENASTEEL is specially designed to replace D2 type steels widely used by toolmakers but suffering from an excessive brittleness. Thanks to its chemistry increasing resistance to softening during tempering, TENASTEEL is especially suited for all processes of surface treatment and coatings commonly used in the market, including nitriding processes involving high temperatures.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Compressive Strength
  • Charpy Impact, Unnotched
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。