Industeel FORA 500 500 HB Wear Resistant Steel

 

Subcategory: Carbon Steel; Medium Carbon Steel; Metal

Material Notes:
Description: FORA 500 is a water quenched martensitic steel, with a 500HB (51.5 HRC), typical hardness, resistant to very severe abrasion wear. Thanks to its mechanical properties, good toughness, high hardness and strength, FORA 500 steel can be used wherever a sliding wear resistance is required and where 400 HB steels do not provide sufficiently long service life. Compared to conventional steels, such as S355, FORA 500 offers a real improvement on the life time of equipment, up to 5 times longer and consequently allows a significant reduction in the design thickness. FORA 500 steel is particularly suitable for applications such as quarries, construction equipment, mines, cement plants, the iron and steel industry, etc.

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Charpy Impact, Notched Low Temp
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。