Subscribe to FREE Trade Publications!

Industeel SUPERPLAST® 400 High Hardness Mold Steel

 

Subcategory: Alloy Steel; Mold Steel

Material Notes:
SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty molds used for production of long series, for compression molds or when an improved wear resistance is expected. SUPERPLAST® 400 will be ideal where a high resistance of the mating plan surface is required and when the conventional 300 HB or even conventional high hard material cannot ensure adapted properties. SUPERPLAST® 400 exhibits processing aptitudes strongly improved compared to conventional steel W1.2711 or equivalent, heat treated to same hardness. This improvement mainly results from a new chemical balance. SUPERPLAST® 400, delivered at 350 to 380 HB, has excellent weldability, a better micro structural homogeneity and a much better machinability than conventional grades heat treated to the same level or even lower hardness.

All injection molds demanding high mechanical properties: long series; high injection series; injection of reinforced plastics (glass fibers); wear problems; compression molds

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。