Johnson Matthey JM A25 Soft Solder/Flux

 

Subcategory: Silver Alloy; Precious Metal; Lead Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materials can be offered as solid wires or as flux cored, to suit the required applications. A wide range of Silver containing solders are suitable for applications where higher strength, increased corrosion resistance or electrical conductivity are required.

In some markets the use of Lead or Cadmium containing solders is prohibited in potable water systems, this has led to the increase use of the Silver bearing and Copper bearing-Lead free solders. Solders are available as: Sticks wire (solid or flux cored), preforms, ingots, ribbon bars and solderpaste.

BS.EN 29453 Alloy No. 32

Information provided by Johnson Matthey.

Available Properties
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。