Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286

 

Subcategory: Superalloy; Stainless Steel; Iron Base; Metal

Key Words: AMS 5525; AMS 5858 (Welding Quality)

Material Notes:
Iron content above calculated as remainder.

Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at high temperatures. Specific uses include jet engine nacelles, parts, and fasteners. Allegheny Ludlum Altemp A286 alloy is a heat and corrosion resistant austenitic iron-base material which can be age hardened o a high strength level. The alloy is also used for low temperature applications requiring a ductile, non-magnetic high strength material at temperatures ranging from above room temperature down to -196 degrees Celsius. The alloy may be used for moderate corrosion applications in aqueous solutions. This alloy can be produced by AOD refining or vacuum induction melting. Vacuum arc or electroslag remelting procedures may be used to further refine the material.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。