Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000

 

Subcategory: Electronic/Magnetic Alloy

Key Words: ASTM A-753; ASTM B-753

Material Notes:
Iron content above calculated as remainder.

The alloy produces good magnetic properties, wide latitude to control hysteresis loop shape via recrystallization modes. Applications for this grade range from electromechanical relay cores, to very low current holding magnets for natural gas safety valves, to manufacture of magnetic shielding used in multiple-wall shielding to produce high frequency transformer applications - notably in the past in telecommunication applications. AL 4750 alloy is sold in two grades, "Rotor" a fine grained, equalized structure with a cube on face texture for rotating equipment, and "Transformer" a large grained directional, secondarily recrystallized twinned structure ideal for transformers.

Information provided by Allegheny Ludlum.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。