Allegheny Ludlum AL 20™ Specialty Steel Alloy (20CB-3), Plate, UNS N08020

 

Subcategory: Superalloy; Stainless Steel; Nickel Base; Metal

Material Notes:
Iron content above calculated as remainder; Nb content above includes Ta.

The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.

Although AL 20 alloy was developed for improved resistance to corrosion by sulfuric acid, it fins wide use throughout the chemical industry. It is used extensively in the manufacture of solvents, explosives, plastics, synthetic fibers, organic chemicals, pharmaceuticals, and food-processing equipment. Containment of acid mixtures and chloride stress corrosion resistance are examples of successful applications for AL 20 alloy. Where purity must be maintained in the processing of products such as foodstuffs or dyes, AL 20 alloy is used to protect end products from the danger of contamination by metallic ions through corrosion.

AL 20 alloy has been applied economically in many areas where other materials my provide the necessary corrosion resistance, but are either higher in initial cost or more expensive to install and maintain. Important advantages of AL 20 alloy are its excellent mechanical properties and comparative ease of fabrication. The presence of columbium in the alloy minimizes the precipitation of carbides in heat-affected zones during welding so that assemblies can usually be placed in service in the as-welded condition. Welds with matching filler metal will be slightly less corrosion resistant than the base alloy.

The N08020 alloy is readily available in a wide range of product forms, and is covered by a wide variety of ASTM and ASME specifications having assigned maximum working stresses to 540 °C. The alloy is familiar to many fabricators and the weldability of this alloy contributes to its use in many engineered applications. Weld filler metal is readily available and welding procedures are well established.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。