Allegheny Ludlum AL Altemp® 625 Nickel-Base Superalloy, UNS N06625

 

Subcategory: Superalloy; Nickel Base

Key Words: DIN 2.4856; ASTM B-443; ASME SB-443; AMS 5599

Material Notes:
Nickel content above calculated as remainder and includes Co.

Allegheny Ludlum Altemp 625 alloy is an austenitic nickel-base superalloy possessing excellent resistance to oxidation and corrosion over a broad range of corrosive conditions, including jet engine environments and in many other aerospace and chemical process applications. Specific uses include jet engine nacelles, engine plumbing, aircraft ducting, recuperators, and thrust reversers. The alloy has outstanding strength and toughness at temperatures ranging form cryogenic temperature to 1093°C. This alloy also has exceptional fatigue resistance.

The Altemp 625 alloy derives its strength from the solid solution strengthening effects of molybdenum and columbium on the nickel-chromium matrix. These elements also contribute to the alloy's outstanding corrosion resistance. Although the alloy was developed for high temperature strength, its highly alloyed composition provides a high level of general corrosion resistance to a wide range of oxidizing and non-molybdenum provide excellent resistance to chloride ion pitting and the high level of nickel provides resistance to chloride stress corrosion cracking.

The material posses a high degree of formability and shows better weldability than many high alloyed nickel-base alloys. The alloy is resistant to intergranular corrosion even in the welded condition.

Information provided by Allegheny Ludlum.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Magnetic Permeability
  • Specific Heat Capacity
  • Melting Point
  • Solidus
  • Liquidus
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。