Allegheny Ludlum AL 825™ Specialty Steel Alloy, UNS N08825

 

Subcategory: Superalloy; Stainless Steel; Nickel Base; Metal

Material Notes:
Iron content above calculated as remainder.

Allegheny Ludlum AL 825 alloy is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of corrosion resistance to both moderately oxidizing and moderately reducing environments. The alloy has a high level of nickel, which in combination with the level of molybdenum and copper, produces substantially improved corrosion resistance in reducing environments compared to the standard stainless steels.

The nickel content is sufficiently high to provide superb resistance to chloride stress corrosion cracking. The chromium and molybdenum content of the alloy provides a level of resistance to chloride ion pitting, however, not to the level of other Allegheny Ludlum alloys. In addition, the alloy is stabilized against sensitization in the welded condition by the addition of a specified level of titanium. Because of this stabilization, the material is resistant to intergranular attack after exposure in the temperature range which would sensitize unstabilized stainless steels.

This alloy has a long history of use in many corrosive environments and has been incorporated in ASTM and ASME specifications for many years.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。