Lucas-Milhaupt BRAZE 403 Carbide Brazing Alloy

 

Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: Braze 403 is a good intermediate temperature brazing alloy for use on stainless steels, mild steels, cast and malleable irons and various nonferrous alloys. This alloy is particularly useful for brazing stainless steel food containers and food handling equipment where a cadmium-free brazing alloy is specified.

Characteristics:Braze 403 is an intermediate temperature silver brazing filler metal with a fairly long (215°F/100°C) melting range. It has a tendency to liquate (i.e. separate into low and high melting constituents) and therefore it is preferable to use this filler metal melting range, or where the assembly can be preheated before the filler metal is applied.

Specifications:This alloy conforms to the following specifications-AWS A5.8 BAg-4, ASME Boiler & Pressure Vessel Code Sec. II C, SFA-5.8 BAg-4

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Tensile Strength, Ultimate at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Shear Strength
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。