Lucas-Milhaupt BRAZE 452

 

Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap applications. (.001-.005" clearance). Handy Flux or Handy Flux Type B-1 should be used with this alloy.

Applications:Braze 452 is a good, general purpose, low temperature filler metal used in cadmium-free brazing applications. It offers an excellent compromise between low melting point and moderate silver content. For improved corrosion resistance in stainless steel joints, use an alloy such as Braze 505 which contains a small amount of nickel.

Specifications:Braze 452 conforms to the following specifications- AWS A5.8 BAg-36

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Elongation at Break
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。