Lucas-Milhaupt BRAZE 051 Silver Based Cadmium Free Filler Metal

 

Subcategory: Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Braze 051 is a low cost, intermediate temperature silver brazing filler metal suitable for joining various ferrous and non-ferrous alloys that can be heated to 1650EF/900EC without damage. The relatively high flow point of this filler metal, combined with its high zinc content, tends to cause a rapid alloying of Braze 051 with non-ferrous alloys. For this reason, the time the brazing alloy is kept molten, in contact with the base metal, should be kept to a minimum. In furnace brazing, the heating cycle should be kept short to avoid excessive volatilization of the zinc with resultant formation of pinholes in the brazing alloy layer.

Applications:The high flow point and narrow melting range of Braze 051 are useful for applications where the brazing and heat treating of ferrous alloys are combined in one operation. The alloy is useful for brazing Nichrome resistance wires because the brazing temperature is high enough to cause stress relief annealing of the Nichrome thus avoiding intergranular cracking.

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。