Lucas-Milhaupt BRAZE 300 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics: Braze 300 is an intermediate temperature silver brazing alloy with a fairly long (160EF/70EC) melting range. This long melting range is helpful when wide gap joints are brazed and is useful in producing large joint fillets to reduce the notch effect in stressed assemblies. Where the higher brazing temperature and characteristics of this alloy are permissible, the lower silver content affords a saving. Handy Flux should be used with this alloy.

Applications:Braze 300 is a good general purpose, intermediate temperature brazing alloy for use on copper, brass, nickel-silver, bronze, steel and other nonferrous alloys melting above 1450EF (765EC). Uses include the brazing of nickel-silver hollow knife handles and electrical equipment. It is particularly adaptable to metal bath dip brazing of fine wires for radio, small transformer and electronics assemblies because its flow point matches the fluid temperature of borax. Borax is used as a metal bath flux cover because it is less corrosive to ceramic pot linings than Handy Flux. Braze 300 exhibits better stability than lower melting alloys when used for metal bath dip brazing.

Specifications:This alloys conforms to the following specifications-AWS A5.8 BAg-20, ASME Boiler & Pressure Vessel Code Sec II-C, SFA-5.8 BAg-20

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Elongation at Break
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  • Corrosion Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。