Lucas-Milhaupt BRAZE 541 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through its melting range. Therefore, it is preferable to use this alloy where the assembly can be heated rapidly to brazing temperature. The long melting range of this alloy is useful when wide gap joints are hand fed since semi-fluid alloys can be worked across the gaps.

Applications:Braze 541 is employed in numerous furnace brazing situations because of its low zinc content. The U.S. Air Force specifies it for many jet engine sub-assemblies. It is used for making joints that are subjected to elevated temperatures, ranging up to 700EF (370EC), particularly on stainless steel.

Specifications: This alloy conforms to the following specifications-AWS A5.8 BAg-13, ASME Boiler & Pressure Vessel Code Sec. II C SFA-5.8 BAg-13, SAE AMS 4772

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Elongation at Break
  • Shear Strength
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。