Lucas-Milhaupt BRAZE 559 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Braze 559 is an intermediate temperature silver brazing alloy similar to Braze 541 (54 Ag, 40Cu, 5 Zn, 1 Ni). It has a rather long melting range (220EF/105EC) so that it will tend to liquate (i.e. separate high from low melting phases) if it is heated slowly through its melting range. However, the long melting range is useful when wide gap joints are brazed as it will bridge the gap and produce larger fillets than alloys with short melting ranges that are more fluid. For torch brazing or furnace brazing with flux it is recommended that Handy Flux type B-1 be used with this alloy.

Applications:Although Braze 559 may be used in flux type brazing, its principal use has been in fluxless brazing of stainless steels in dry hydrogem atmosphere. Braze 559 is free of zinc and it would have an advantage over Braze 541 in fluxless furnace brazing applications where zinc volatilization is objectionable.

Specifications: Braze 559 conforms to the following specifications-AWS A5.8 BAg-13a, ASME Boiler & Pressure Vessel Code Sec. II C SFA-5.8 BAg-13a, SAE AMS 4765

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。