Lucas-Milhaupt BRAZE 580 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Braze 580 is a free flowing intermediate temperature cadmium-free silver brazing filler metal that exhibits an unusual ability to wet certain base metals that are difficult to braze with more standard alloys. Typical of these base metals are chromium and tungsten carbides. Unlike some other manganese containing brazing filler metals, Braze 580 does not tend to produce porous fillets. Braze 580 contains no zinc or cadmium and will not outgas during Titanium Nitride coating of tools.

Applications:This alloy should be regarded as a special purpose material for brazing difficult to wet metals and alloys such as tungsten and chromium carbides. Wetting studies show that this alloy exhibits excellent wetting in vacuum brazing of high manganese stainless steels. For details consult: Vacuum Brazing of High Manganese Stainless Steel by W. S. Bennett and R.F. Hillyer, Welding Journal (Vol 53, No. 11, Nov. 1974, P510S).

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。