Lucas-Milhaupt BRAZE 630 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics: Braze 630 is very sluggish because of its wide melting range, and will bridge wide or irregular joint clearances. To avoid liquation (separation and flow of the low-melting components) the joint and alloy preplacement should be designed for a minimum distance of flow (i.e., preplaced sheet-preforms), particularly when slow heating will occur through the melting range. Fast-heating or application of the alloy after the joint is at temperature will minimize liquation. Heating the assemblies above 1700°F (925°C), as in brazing/heat-treatment, will improve the fluidity of the brazing alloy and accelerate the heating rate in the alloy melting range.

Handy Flux is usually recommended for use with Braze 630 when brazing the 400 series stainless steels with torch, air-gas burner, or RF induction coil. Joint clearances of 0.002" - 0.010" (5-25 mm) are recommended. Better flow could be obtained with Handy Flux Type B-1, but this improvement would reduce corrosion resistance of the joint at fillet edges.

Braze 630 can be used in protective atmosphere (including vacuum) furnace brazing without flux. Excellent joints with good smooth fillets can be obtained on stainless steels at furnace temperatures of 1700 - 1850°F with a H2N2 atmosphere having a dew point of -50°F or lower and joint clearances of 0.002" - 0.007" (.05-.18mm).

Applications: Braze 630 is a low temperature brazing filler metal developed for use on 400 series stainless steels for maximum resistance to interface corrosion. It can be used on 200, 300, and 400 series stainless steels and other alloys for combined brazing/heat treatment with flux, or in protective atmosphere (including vacuum) furnaces. It is used in vacuum applications, and in joints where greater oxidation resistance than the other silver brazing alloys is required. It is also used in surgical and food-handling equipment requiring cadmium-free alloys.

Braze 630 can be used on joints exposed to conditions favoring dezincification of zinc-coating alloys such as salt-water at elevated temperatures.

Specifications: This alloy conforms to the following specifications- AWS A5.8 BAg-21, SAE AMS 4774, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-21

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。