Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wetting and bonding. In brazing gray cast iron it is necessary to treat the surface prior to brazing to remove graphite, in order to assure good wetting by the brazing filler metal.

A complete list of the uses of Easy-Flo 45 would include practically all applications for which silver brazing filler metals have been used.

Characteristics: Easy-Flo 45 is a eutectic type, free-flowing filler metals that, because of their narrow melting range, are less sensitive to the rate of heating and should not liquate (i.e. separate into low and high melting constituents). This high fluidity makes well-fitted joints essential and prevents bridging or large fillet formation. Handy Flux should be used with either of these filler metals.

Some base metals when brazed under high stress may crack during brazing when the stressed base metal is wetted by the brazing filler metal. This is a form of stress corrosion cracking. The low flow temperature of Easy-Flo is below the stress relaxation temperature of some nickel base alloys. The cure is to relieve the stress before the brazing alloy is applied. A higher melting brazing filler metal may be preferred since stress relief will then occur before the filler metal melts.

Specifications:This filler metal conform to the following specifications: AWS A5.8 BAg-1, SAE-AMS 4769, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-1

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Tensile Strength, Ultimate at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。