Lucas-Milhaupt EASY FLO 30 Silver Based Cadmium-Bearing Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: Easy-Flo 30 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrousand nonferrous metals. Because of their fairly low cost, good fatigue strength and ability to make leak-tight joints where close clearances cannot be maintained, they have been widely used in the refrigeration and air-conditioning industry. Additional uses for these filler metals are tubular bicycle and furniture frames, where joint fitup may be variable.

Characteristics: Easy-Flo 30 is a low temperature, economical, brazing filler metals capable of bridging gaps where poor jointfitup cannot be avoided. This filler metal has a tendency to liquate (i.e., separate into low and high melting constituents)when heated slowly and therefore it is preferable to use them where the heat source is sufficient to raise the part temperaturerapidly through the melting range of the brazing filler meta. Handy Flux is recommended for use with this filler metal.

Specifications:This filler metal conform to the following specifications: AWS A5.8 BAg-2a, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-2a

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。