Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy

 

Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning apparatus, electrical conductors, copper and brass pipe fittings, and other copper and brass equipment.

Characteristics: Sil-Fos is copper rich, filler metals that are self-fluxing on copper by virtue of their phosphorus content. Sil-Fos, because of its higher phosphorus content, is more fluid than Sil-Fos 5 when heated rapidly to its flow point. Sil-Fos has less tendency to form large fillets or to fill poorly fitted joints with large clearances cannot be maintained or where fillets are specified.

The self-fluxing of these filler metals is effective on copper only. With copper-base alloys, such as bass or bronze, the joints should be fluxed with Handy-Flux. Sil-Fos should not be used on nickel-base alloys, as the phosphorus reacts with the nickel or iron to form brittle compounds at the interface of the joints.

Both Sil-Fos is mutually soluble with copper and copper alloy base metals.

This metal has a strong tendency to liquate (i.e. to separate into low and high melting constituents) if heated slowly through its melting range, as normally occurs in furnace brazing. The results in leaving a skull of unmelted alloy behind which may objectionable from the standpoint of appearance. In furnace brazing it is preferable to preplace the alloys inside the joint where the skull is not visible.

Specifications:This filler metal conform to the following specifications:AWS A5.8 BCuP-5, ASME Boiler & Pressure Vessel Code, Sec II-C, SFA5.8 BCuP-5

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Specific Gravity
  • Density
  • Tensile Strength @ Break
  • Tensile Strength, Ultimate at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。