MetaFoam® Copper Foams

 

Subcategory: Copper Alloy; Metal

Material Notes:
General Description:

MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional” metal foams. MetaFoam can significantly increase specific surface area and repetability, while maintaining the lowest production costs. MetaFoam is uniquely positioned to develop products and address several needs in various industries and markets.

Applications:

There are plenty of flieds of applications for open-cell metal foams, including:

  • Thermal management and heat transfer
  • Electrochemistry and catalysts
  • Water and air purification/filtration
  • Biomedical implants
  • Flow control devices
  • Acoustic
For now, MetaFoam is focusing on particular applications:
  • Metal foam wicking structure for cylindrical, flat, and loop heat pipes that perform in any orientation
  • Cold plates with a metal foam core for electronics cooling without the high cost of micromatching
  • High surface area boiling / evaporator plates for increased critical heat fluxes
  • High surface area porous electrodes to increase electrochemical reaction efficiency
  • Water purification with copper-silver foams, two metals having renowned properties against bacteria and algae.

Available Properties
  • Porosity
  • Permeability
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Nusselt Number in Air
  • Pores diameter, mm
  • slabs size, cm
  • slabs thickness, mm
  • Sound Absorption
  • Sound Reduction
  • Surface Area, m^2/m^3
  • Tortuosity
  • Windows diameter, µm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。