Plansee PM 1000 ODS Nickel Alloy

 

Subcategory: Superalloy; Metal Matrix Composite; Nickel Alloy; Nonferrous Metal

Close Analogs: Nickel content calculated as remainder.

Key Words: Grain Class 16; Material No. 2.4869; Abbreviated DIN Name: NiCr 80/20; Oxide Dispersion Strengthened

Material Notes:
PM 1000 is a cold-workable oxide dispersion strengthened (ODS) Ni based material with a high chromium alloy content. Dispersion strengthening with nano sized Y2O3 particles in combination with recrystallised coarse grained microstructure gives PM 1000 highest tensile and rupture strength at high temperatures. With a chromium content of 20% the material also shows excellent hot corrosion properties.

Advantages of PM 1000:

  • excellent creep strength up to 1200°C
  • hot gas corrosion resistant up to 1200 °C
  • superior low cycle fatigue properties
  • optimised emissivity properties for space applications up to 1300°C
Typical fields of application for PM 1000:
  • pull rod assemblies for high temperature testing
  • punches for the hot pressing of diamond containing tooling
  • hot metallic structures for the aerospace industry
  • guide vanes for gas turbines
  • spinner rings for the glass and ceramics industry
Information provided by Schwarzkopf Technologies, a Plansee Affiliated Company.

Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Modulus of Elasticity
  • Impact
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。