Plansee PM 2000 Grain Class 6 ODS Iron Alloy Bar

 

Subcategory: Superalloy; Metal Matrix Composite

Close Analogs: Iron content calculated as remainder.

Key Words: Material No. 1.4768; Abbreviated DIN Name CrAl 21 6; Oxide Dispersion Strengthened

Material Notes:
The PLANSEE sophisticated PM 2000 is a highly oxidation resistant and extremly creep resistant ferritic iron-chromium based alloy. Homongenious dispersion strengthening with nano sized Y2O3 particles in combination with recrystallised coarse grained microstructure gives PM 2000 highest hot strength and creep strength up to 1350°C. Due to its high content of Aluminium and Chromium, PM2000 forms a dense and adherent Al2O3 scale when used at high temperatures under oxidising atmospheres. This oxide scale is highly resistant to high-speed gas flows up to 1300°C.

Advantages of PM 2000:

  • extraordinary creep resistance up to 1350 °C
  • high hot strength up to 1300°C
  • excellent oxidation and hot corrosion resistance
  • highly resistant against coking and carburisation compared to NiCr alloys
  • due to its lower density, components made from PM 2000 are lighter than those made from Ni base materials
  • high stability against high-speed gas flows at temperatures up to 1300 °C
  • good machinability with normal tooling
Typical fields of application for PM 2000:
  • thermocouple sleeves for high temperatures
  • burner nozzles
  • charge carriers for parts for high temperature furnace construction
  • pull rod assemblies for high temperature testing
  • stirrers for the glass industry
  • honey comb structures for aerospace
  • components for the chemical plant construction
  • combustion parts for engines

Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Fracture Toughness
  • Impact
  • Electrical Resistivity
  • Magnetic Coercive Force, Hc
  • Curie Temperature
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。