Sandvik 6UF Ultra-fine Grain Cemented Carbide for Printed Circuit Board Printing

 

Subcategory: Metal Matrix Composite; Carbide; Tungsten Alloy; Nonferrous Metal

Material Notes:
SANDVIK ultra-fine grain cemented carbide grades are the result of an extensive development programme, aimed at optimising the very best of cemented carbide technology to achieve an exceptional combination of hardness, toughness and strength.

These extraordinary properties have been achieved by producing tungsten carbide with a grain size of only 0.4 µm. In addition, a special additive maximises corrosion resistance without loss of toughness.

SANDVIK ultra-fine grain cemented carbide grades have been developed to meet the latest demands, placed on solid carbide tooling by modern technology.

SANDVIK grade 6UF incorporates 6% cobalt (Co) and 94% tung sten carbide (WC).

6UF is recommended for solid carbide rotary tool applications in the ISO K01/K05 range where high cutting speeds are possible.

Information provided by Sandvik

Available Properties
  • Density
  • Hardness, Rockwell A
  • Hardness, Vickers
  • Rupture Strength
  • Compressive Strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。