Sandvik KANTHAL Kanthal D Resistance Ribbon

 

Subcategory: Aluminum Alloy; Iron Base; Metal

Material Notes:
KANTHAL D is a ferritic FeCrAl alloy which is used at wire temperatures up to 1300°C (2370°F). It is used in domestic appliances as well as in industrial applications.

Typical applications for KANTHAL D are in metal sheathed tubular elements for dishwashers, in elements embedded in ceramics forpanel heaters, in cartridge elements in metal dies, in heating cables and rope heaters in defrosting and de-icing elements, in mica elements used in irons, in quartz tube heaters for space heating, industrial infrared dryers, in coils on molded ceramic fibre for boiling plates with ceramic hobs, in bead insulated coils for panel heaters, in suspended coil elements for air heaters in laundry dryers. In industrial applications such as terminals to furnace elements, in porcupine elements for air heating, and in furnace heating elements.

Information provided by Sandvik

Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Elongation at Break
  • Creep Strength
  • Modulus of Elasticity
  • Poissons Ratio
  • Electrical Resistivity
  • Curie Temperature
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Emissivity (0-1)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。