MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Sandvik 2002 Precision Wire

 

Subcategory: Stainless Steel; Alloy Steel; Metal; Ferritic

Material Notes:
Sandvik 2002 is a ferritic stainless steel used for length turning automatics. Special applications are fine mechanicals and electronics there magnetical material can be used.

Sandvik 2002 has very good cutting properties both at low and high cutting speeds. Material gives low wear on tools at machining on high speed steel and hard metals. This gives very high precision on final products and possibilities to increase cutting speeds and improve productivity.

Very good machining properties and the corrosion resistance is equal to or better than material of type SS2346. Resistivity against general corrosion is very good.

Sandvik 2002 has cold deformation properties equal to Sandvik 1802.

Service temperature -60 to 300°C. Long time use at elevated temperatures gives brittleness.

Information provided by Sandvik

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Charpy Impact
  • Electrical Resistivity
  • Magnetic Permeability
  • Magnetic Coercive Force, Hc
  • Magnetic Saturation Flux Density, Bmax
  • Magnetic Remanence, Br
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Transformation Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。