Sandvik Bioline 1RK91 Precision Wire

 

Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal; Ferritic

Material Notes:
Sandvik Bioline 1RK91 (a Sandvik NanoflexTM material) is a precipitation hardening stainless steel grade specifically designed for applications requiring high strength combined with good ductility in the final product and high formability in the as-delivered condition. The strength is increased after ageing of the final product.

The characteristics in general can be said to be a combination of properties of ordinary austenitic stainless and low alloyed ferritic steels. This means that properties such as elastic modulus, mechanical properties and thermal expansion are comparable to ferritic steels (such as low alloyed carbon steels or chromium steels) while properties such as corrosion resistance is more comparable to austenitic stainless steels.

  • excellent mechanical properties, very high tensile strength and hardness levels can be achieved
  • corrosion resistance comparable to AISI 304L or AISI 316L depending on condition
  • retained mechanical properties at temperatures up to at least 400oC good weldability
  • Information provided by Sandvik

    Available Properties
    • Density
    • Tensile Strength, Ultimate
    • Tensile Strength, Ultimate at Elevated Temperature
    • Tensile Strength, Yield
    • Modulus of Elasticity
    • CTE, linear 100°C
    • CTE, linear 250°C
    • CTE, linear 500°C
    • Specific Heat Capacity
    • Thermal Conductivity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。