Sandvik Sanicro 69 Seamless tube and pipe

 

Subcategory: Nickel Alloy; Metal

Close Analogs: UNS N06690; EN 2.4642

Material Notes:
Austenitic nickel-chromium-iron alloy, UNS N06690

Sandvik Sanicro 69 is an austenitic nickel-chromium-iron alloy used primarily for steam generators in nuclear power plants (PWR). For this application it is used in the "thermally treated" condition. This treatment results in chromium carbide precipitation at the grain boundaries but no significant chromium depletion.

For the steam generator application the material is characterised by:

  • extremely high resistance against stress corrosion cracking in primary side PWR water conditions
  • improved pitting corrosion resistance in chloride containing solutions compared with Alloy 600
  • good corrosion resistance in caustic environments
  • For other applications the material is characterised by:

  • excellent performance in nitric acid solutions
  • very good resistance against high temperature oxidation
  • The material has also:

  • good structure stability
  • good weldability
  • Information provided by Sandvik

    Available Properties
    • Density
    • Hardness, Vickers
    • Tensile Strength, Ultimate
    • Tensile Strength, Ultimate at Elevated Temperature
    • Tensile Strength, Yield
    • Tensile Strength, Yield at Elevated Temperature
    • Elongation at Break
    • Modulus of Elasticity
    • Electrical Resistivity
    • CTE, linear 100°C
    • CTE, linear 250°C
    • CTE, linear 500°C
    • Specific Heat Capacity
    • Thermal Conductivity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。