Stoody® 19 Cobalt-Base Cast Alloy

 

Subcategory: Superalloy; Nonferrous Metal; Cobalt Base

Key Words: MIL-C-24248; Deloro Stellite Inc.

Material Notes:
Cobalt content above calculated as balance.

Stoody® 19 is a cobalt-base centrifugally cast alloy roughly intermediate in alloy content and properties between stoody 12 and stoody 3. It is close in composition and hardness to Stoody 1, differing primarily in its slightly higher chromium content and slightly lower tungsten content. This alloy can be certified to meet the requirements of MIL-C-24248 (ships) Composition III.

Recommended for guide rolls, thrust bearing shoes, ball bearing races.

Information provided by Deloro Stellite Inc.

Available Properties
  • Hardness, Rockwell C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。