Stellite® alloy 6B, solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate, tested at 538°C (1000°F)

 

Subcategory: Superalloy; Cobalt Base

Key Words: Deloro Stellite Inc.

Material Notes:
Cobalt content as balance. Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and cement and steel-mill equipment. Resistant to the effects of seizing or galling, low coefficient of friction alloys sliding contact with other metals. Used in equipment where no lubricants are used. Outstanding resistance to cavitation-erosion. Combines wear and corrosion resistance with good impact strength and resistance to thermal shock. Retains high hardness, even at red heat. Electrical conductivity 1.90% compared to Copper. 2360 MPa average modulus of rupture of sheet at room temperature.Data provided by the manufacturer, Deloro Stellite, Inc.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell A
  • Hardness, Rockwell B
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Charpy Impact
  • Charpy Impact, Unnotched
  • Izod Impact Unnotched
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Reflection Coefficient, Visible (0-1)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。