Stellite® alloy 19

 

Subcategory: Superalloy; Cobalt Base

Close Analogs: Stoody 1, Stoody 5

Key Words: MIL-C-24248 Comp II

Material Notes:
Cobalt content as balance. Can be machined with carbide tipped tools, but when hardness exceeds Rc55 it is best to grind. Applications include cutting tools, bearing races, guide rolls, and nozzle discs. Excellent resistance to hot abrasion and adhesive wear, low coefficient of friction. Resistant to atmospheric oxidation and forms only a thin adherent scale at red heat. Resists attack from wet chlorine and acetic acid (boiling), excellent resistance to 10% boiling nitric, and 10% sulfuric acid at room temperature. Fair resistance to concentrated nitric boiling and 10% boiling sulfuric. Poor resistance to 77% sulfuric boiling and reducing acids.Data provided by the manufacturer, Deloro Stellite, Inc.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Ultimate Compressive Strength
  • Izod Impact Unnotched
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。