BryCoat Thermal Spray Coatings

 

Material Notes:
Thermal spray coatings are applied by spraying fine powdered materials to the part surface at extremely high velocities. The resulting coatings can be from 0.0005 inches to over 0.100 inches. Thermal spray coatings are used for

  • Wear Resistance
  • Corrosion Resistance
  • Abrasion Resistance
  • Dimensional Restoration
  • Thermal Barrier
Many different coating materials can be used, such as ceramics, MCrAlYs, carbides, oxides, and alloys. Coating systems include HVOF (High Velocity Oxy Fuel) and High Energy Air Plasma.

Attributes of plasma spray coating:

  • Cost Effective
  • Good Wear Factor
  • Bond Tensile Strength (6000 psi typical)
  • High Density (15% porosity)
  • Excellent for Thermal Barrier Coatings (TBCs)
Attributes of HVOF Coating:
  • Excellent Wear Factor
  • Very High Density (1% porosity)
  • Outstanding Adhesion
  • Bond Tensile Strength (15,000 psi typical)

Information provided by BryCoat, Inc.

Available Properties

We're sorry, but our sources do not report
any other information for this material.

  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。