Latrobe Lescalloy® D6AC VAC-ARC High Strength Alloy Steel

 

Subcategory: Low Alloy Steel; Medium Carbon Steel; Metal

Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Material Notes:
LESCALLOY D6AC VAC-ARC steel is a medium carbon, low alloy, ultra high strength steel primarily designed for high strength structural applications requiring strength leaves up to 280,000 psi. This alloy provides a high yield strength to tensile strength ratio, combined with good ductility. A tough and fibrous fracture is exhibited to as low as -210°F in impact testing; also the notch toughness is excellent. It has been selected for fracture toughness critical applications at a variety of strength levels. The deep hardening characteristics of D6AC steel make it applicable for fairly large sections. Lescalloy D6AC VAC-ARC steel is produced by the consumable electrode vacuum arc remelting process to provide optimum cleanliness and preferred ingot structure, which in turn provide optimum transverse mechanical properties.

Heat Treatment - Austenitized at 1650°F. Oil quenched and air cooled, or salt quenched at 400-425°F for 10 minutes and air cooled

Information Provided by Timken Latrobe Steel.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Ultimate Tensile Strength
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Machinability
  • CTE, linear 20°C
  • CTE, linear 500°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。