Latrobe Stark™ ASTM M4 High Speed Steel

 

Subcategory: Tool Steel; High Carbon Steel; Alloy Steel; Metal

Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Material Notes:
STARK (M4) is a super high speed steel with very high carbon and vanadium contents for exceptional abrasion resistance. It is well suited for premium cutting tools of all types, particularly those used for machining abrasive alloys, castings, and heat-treated materials. The high carbon content enables Stark to be hardened in excess of 65 HRC. However, the high hardness and high vanadium carbide content make Stark more difficult to grind after heat treatment compared to Double Six (M2) and other high speed steels. Typical applications for Stark high speed steel include form tools, spade drills, end mills, taps and dies, punches and broach inserts.

Information Provided by Timken Latrobe Steel.

Available Properties
  • Specific Gravity
  • Density
  • Critical Temperature
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Izod Impact Unnotched
  • Machinability
  • CTE, linear 20°C
  • CTE, linear 500°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。