Latrobe LSS™ 135M Nitriding Steel (ASTM A355 Class A)

 

Subcategory: Medium Carbon Steel; Alloy Steel; Metal

Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Material Notes:
TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured from this steel are surface nitrided. The result is a nitrided surface which exhibits high hardness and good resistance to abrasion and wear, along with a strong and tough inner core in the piece. TLS 135M is supplied in the prehardened condition at a hardness of approximately 28 to 32 Rockwell C. In this condition, tools can be machined or ground, and then nitrided. Additional heat treatment is normally not required. Typical applications for TLS 135M steel include injection and extrusion feed screws, machine parts, pump parts, bushings, shafts, pinions, crankshafts, cams, camshafts, gears, valve sleeves, chuck jaws, dowel pins, and thread guides.

Information Provided by Timken Latrobe Steel.

Available Properties
  • Specific Gravity
  • Density
  • Hardness, Rockwell C
  • Ultimate Tensile Strength
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Machinability
  • CTE, linear 20°C
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。