Latrobe LSS™ 420 MQ Plastic Mold Steel (AISI 420)

 

Subcategory: Stainless Steel; Mold Steel; Metal

Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Material Notes:
TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an electric-arc furnace, is refined by the argon-oxygendecarburization (AOD) process, and is further enhanced to aerospace quality levels using Vacuum-Arc or Electro-Slag Remelting. These special melting and forging practices result in ultra-high microcleanliness and a homogeneous microstructure. TLS 420 MQ is a superior material for the manufacture of plastic molds that require high hardness for good parting line retention and sealing between colored resins. It also resists attack from the corrosive vapors that are produced during molding of some plastic resins. The corrosion resistance also enhances extended tool storage in humid environments. The high cleanliness and homogeneity make TLS 420 MQ a superb choice for mold cavities that require photoetching/texturizing or the highest, lens-quality polished finishes. T

Available Properties
  • Specific Gravity
  • Density
  • Critical Temperature
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Izod Impact Unnotched
  • Machinability
  • CTE, linear 20°C
  • CTE, linear 500°C
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。