Universal Wire Works 347 Stainless Steel Electrode

 

Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal

Key Words: AWS E347-15,16

Material Notes:
Iron content is calculated as remainder.

Universal 347 electrodes were developed for the welding of types 321 and 347 stainless and the clad side of steel clad with like alloys. Alloy 347 is used for the fabrication of equipment, which must be placed in service under severe corrosive conditions. Typical applications include pressure vessels for continuous service at temperatures of 700 to 1600 degrees F such as chemical plant and oil refinery equipment. Alloy 347 electrodes are columbium stabilized, containing columbium in the amount of 10 times the amount of carbon with a maximum of 1.00%. When welding stabilized alloys of 321 and 347, intergranular corrosion does not occur.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Available Properties
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。