Universal Wire Works 55 Nickel Alloy Welding Wire

 

Subcategory: Nickel Alloy; Nonferrous Metal

Key Words: AWS A5.15 Class ENiFe-Cl

Material Notes:
Universal nickel alloy 55 is designed to arc weld cast iron, malleable iron, ductile iron, and Ni-Resist as well as welding cast irons to steel and high nickel alloys. Alloy 55 is also used for welding high phosphorous irons and casting that have heavy for thick sections. Castings can be welded without preheat, however a more machinable deposit and less stresses will be built up in the welding zone if a preheat of 400 degrees is used. Alloy 55 can be used in all positions with either AC or DCRP.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Available Properties

We're sorry, but our sources do not report
any other information for this material.

  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。