Universal Wire Works C-276 Nickel Alloy Welding Wire

 

Subcategory: Nickel Alloy; Nonferrous Metal

Key Words: AWS A5.11 / A5.14 Class ENiCrMo-4; ASME

Material Notes:
Nickel content is calculated as remainder.

Alloy C-276 is a low carbon, nickel base alloy containing significant amounts of molybdenum and chromium. Alloy C-276 is one of the most universally corrosion resistant alloys available. This alloy resists the formation of grain-boundary precipitates in the weld heat affected zone, thus making it suitable for most chemical process applications in the as welded condition. Alloy C-276 has exceptional resistance to strong oxidizing agents such as ferric and cupric chlorides, hot contaminated mineral acids, acetic anhydride, and sea water and brine solutions. Alloy C-276 is known to resist the corrosive effects of wet chlorine gas, hypochlorite, and chlorine dioxide solutions. Alloy C-276 is resistant to oxidizing and reducing the atmospheres up to 1900 degrees F and is particularly useful where parts are either highly stressed, or subject to repeated thermal shock at temperatures from 1600 to 1800 degrees F, which makes this alloy useful for hot metal handling equipment and forging hammers and rings.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Available Properties
  • Tensile Strength, Ultimate
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。