Universal Wire Works E81T1-Ni2 Flux Cored Carbon Steel Tubular Electrode

 

Subcategory: Carbon Steel; Metal

Key Words: AWS A5.29 E81T1-Ni2; ASME SFA-5.29 E81T1-Ni2

Material Notes:
Iron content is calculated as remainder.

Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multiple pass welding have a spray-like transfer with very little spatter. The fast freezing slag facilitates welding in all positions and is easily removed. Alloy 81T1-Ni1 is formulated for welding ASTM A572, A302, A588, and A734. These steels are used in the fabrication of transmission poles, light poles, earth moving and mining machinery and offshore platforms. Alloy 81T1-Ni2 is formulated for welding ASTM A572, A575, and A734. The combination of strength and CVN toughness of Ni-2 make it ideal for applications such as offshore platform construction, shipbuilding, earthmoving and mining equipment.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Available Properties
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Charpy Impact, Notched Low Temp
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。