COLMONOY® 57 PTA - Nickel-Base Hard-Surfacing Alloy

 

Subcategory: Metal Matrix Composite; Nickel Alloy; Tungsten Alloy; Nonferrous Metal; Nickel Base

Close Analogs: Nickel content calculated as balance.

Material Notes:
Description: Colmonoy 57 PTA is a unique Ni-Cr-B alloy containing optimized amounts of precipitated tungsten rich hard phases distributed throughout the matrix. These hard phases offer substantial increase in abrasion resistance and reduce the sensitivity of the material to hardness variations during deposition of overlays using PTA equipment. These hard phases are incorporated in the matrix material by careful alloying during the powder manufacturing process, as opposed to external additions in conventional composite powders.

Applications: Colmonoy 57PTA is specifically formulated for overlaying the flights of new and rebuilt extrusion or injection molding screws. It exhibits excellent weldability and is easy for the operator to control. Laboratory tests have shown that variations in PTA deposition parameters have minimal effects on the hardness of the deposit. The alloy also has many other potential applications where resistance to abrasion and corrosion are important. Examples include applications in the food processing industry such as feed screws, air locks and scraper blades.

Information provided by Wall Colmonoy Corporation.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Solidus
  • Liquidus
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。