Quadrant EPP Nylatron® GS Nylon, Type 66, MoS2 filled, extruded

 

Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer; Filled/Reinforced Thermoplastic

Key Words: Polyamide 66; PA66; PA 66; Polyamide 6/6; Polyamide 6,6; Nylon 6/6; Nylon 6,6

Material Notes:
Nylatron GS Nylon is a nylon and molybdenum disulphide (MoS2) composition designed to improve the mechanical, thermal and bearing properties of type 6/6 nylon while maintaining its basic electrical and chemical characteristics. Through compounding, finely divided particles impart extra lubricity to this nylon, permitting Nylatron GS parts to operate with little or no lubrication. The added lubricity also contributes dramatically to component service life, making Nylatron GS a very cost-efficient choice. Nylatron GS nylon offers greater wear resistance, lower surface friction, higher strength and greater rigidity than unfilled 6/6 with improved dimensional stability.

Data provided by Quadrant Engineering Plastic Products.

Available Properties
  • Cost, 1 to 10 (Nylon = 2)
  • Specific Gravity
  • Water Absorption
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Hardness, Rockwell R
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Strength
  • Compressive Modulus
  • Machinability (1-10; 1 = easiest)
  • Dimensional Stability (1-4; 4 = highest)
  • Shear Strength
  • Coefficient of Friction
  • K (wear) Factor
  • Limiting Pressure Velocity
  • Izod Impact, Notched
  • Surface Resistivity per Square
  • Dielectric Strength
  • CTE, linear 68°F
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Grey
  • Acetaldehyde Aq. (40%)
  • Acetamide Aq. (50%)
  • Acetic Acid Aq. (10%)
  • Acetone
  • Acrylonitrile
  • Alcohols, Aliphatic
  • Allyl Alcohol
  • Aluminum Chloride Aq. (10%)
  • Aluminum Sulfate Aq. (10%)
  • Ammonia Aq. (10%)
  • Ammonia Gas
  • Ammonium Carbonate Aq. (10%)
  • Ammonium Chloride Aq. (10%)
  • Ammonium Chloride Aq. (37%)
  • Amyl Acetate
  • Amyl Alcohol
  • Aniline
  • Antimony Trichloride Aq. (10%)
  • Barium Chloride Aq. (10%)
  • Barium Sulfate Aq. (10%)
  • Benzaldehyde
  • Benzene
  • Benzoic Acid Aq. (SAT)
  • Benzyl Alcohol
  • Beverages Aq. Alcoholic
  • Beverages Aq. Carbonated
  • Bitumen
  • Bleaching Lye (10%)
  • Bleaching Lye (100%)
  • Boric Acid Aq. (10%)
  • Boron Trifluoride
  • Bromine Aq. (30%)
  • Bromine Liq.
  • Butanol
  • Butyl Acetate
  • Butylene Glycol
  • Butyric Acid (CONC)
  • Butyric Acid Aq. (20%)
  • Butyrolactone
  • Calcium Chloride (in Alcohol) (20%)
  • Calcium Chloride Aq. (10%)
  • Calcium Hypochlorite
  • Camphor
  • Carbon Disulphide
  • Carbon Tetrachloride
  • Carnalite Aq. (10%)
  • Catechol
  • Chloral Hydrate
  • Chlorine Aq. (10%)
  • Chlorine Gas (100%)
  • Chloroacetic Acid Aq. (10%)
  • Chlorobenzene
  • Chloroform
  • Chlorosulfonic Acid Aq. (10%)
  • Chromic Acid Aq. (1%)
  • Citric Acid Aq. (10%)
  • Citric Acid Aq. (SAT)
  • Coconut Oil
  • Cresols
  • Cupric Sulfate Aq. (0.5%)
  • Cupric Sulfate Aq. (SAT)
  • Cyclohexane
  • Cyclohexanol
  • Cyclohexanone
  • Decalin
  • Detergents, Organic
  • Dibutylphthalate
  • Dichlorodifluoro Methane
  • Dichloroethylene
  • Diesel Oil
  • Diethyleneglycol Aq. (90%)
  • Dimethyl Carbinol
  • Dimethyl Formamide
  • Dioxane
  • Edible Oils
  • Ethanol, Denatured (96%)
  • Ether, Diethyl
  • Ethyl Acetate
  • Ethyl Chloride
  • Ethylene Chloride
  • Ethylene Diamine
  • Ethylene Glycol Aq. (96%)
  • Ferric Chloride Aq. (5%)
  • Ferric Chloride Aq. (SAT)
  • Ferrous Chloride Aq. (10%)
  • Fluorine (Gas Wet)
  • Fluorosilicic Acid Aq.
  • Fluothane
  • Formaldehyde Aq. (10%)
  • Formic Acid Aq. (10%)
  • Formic Acid Aq. (3%)
  • Freon 12 (Arcton 12)
  • Fruit Juices (CONC)
  • Furfural
  • Gasoline
  • Glycerine
  • Heptane
  • Hexane
  • Hydrobromic Acid Aq. (10%)
  • Hydrochloric Acid Aq. (0.4%)
  • Hydrochloric Acid Aq. (10%)
  • Hydrochloric Acid Aq. (2%)
  • Hydrofluoric Acid Aq. (4%)
  • Hydrogen Peroxide Aq. (1%)
  • Hydrogen Peroxide Aq. (3%)
  • Hydrogen Sulfide Aq. (SAT)
  • Hydrogenated Vegetable Oils
  • Hydroquinone
  • Iodine (3%)
  • Iodine (in Alcohol)
  • Iso octane
  • Isopropyl alcohol
  • Isopropyl Ether
  • Lactic Acid Aq. (10%)
  • Lactic Acid Aq. (90%)
  • Lead Acetate Aq. (10%)
  • Lead Stearate
  • Linseed Oil
  • Lithium Bromide Aq. (50%)
  • Lubricating Oils (Petroleum)
  • Magnesium Chloride Aq. (10%)
  • Magnesium Hydroxide Aq. (10%)
  • Magnesium Sulfide Aq. (10%)
  • Maleic Acid Aq. (CONC)
  • Malonic Acid Aq. (CONC)
  • Manganese Sulfate Aq. (10%)
  • Mercuric Chloride Aq. (6%)
  • Mercury
  • Methanol
  • Methyl Acetate
  • Methyl Ethyl Ketone
  • Methylene Chloride
  • Methylpyrrolidone
  • Milk
  • Mineral Oils
  • Naphthalene
  • Nickel Sulfate Aq. (10%)
  • Nicotine
  • Nitric Acid Aq. (0.1%)
  • Nitric Acid Aq. (10%)
  • Nitrobenzene
  • Nitromethane
  • Oleic Acid
  • Oxalic Acid Aq. (10%)
  • Ozone
  • Paraffin
  • Perchloric Acid Aq. (10%)
  • Perchloroethylene
  • Petroleum Ether
  • Phenol (Molten)
  • Phenol Aq. (6%)
  • Phenol Aq. (75%)
  • Phosphoric Acid Aq (0.3%)
  • Phosphoric Acid Aq (3%)
  • Phosphoric Acid Aq. (10%)
  • Phthalic Acid Aq. (SAT)
  • Phthalic Dioctyl
  • Potassium Acetate Aq. (50%)
  • Potassium Bicarbonate Aq. (60%)
  • Potassium Bromide Aq. (10%)
  • Potassium Carbonate Aq. (60%)
  • Potassium Chloride Aq. (90%)
  • Potassium Dichromate Aq. (5%)
  • Potassium Ferricyanide Aq. (30%)
  • Potassium Ferrocyanide Aq. (30%)
  • Potassium Hydroxide Aq. (10%)
  • Potassium Hydroxide Aq. (50%)
  • Potassium Nitrate Aq. (10%)
  • Potassium Permanganate Aq. (1%)
  • Potassium Sulfite Aq. (CONC)
  • Propane Gas
  • Pyridine
  • Resorcinol
  • Salicylic Acid
  • Silicone Fluids
  • Silver Nitrate
  • Soap Solutions
  • Sodium Acetate Aq. (60%)
  • Sodium Bicarbonate Aq. (50%)
  • Sodium Bisulphite Aq. (10%)
  • Sodium Bromide Aq. (10%)
  • Sodium Carbonate Aq. (20%)
  • Sodium Chlorate Aq. (10%)
  • Sodium Chloride Aq. (10%)
  • Sodium Chloride Aq. (90%)
  • Sodium Hydroxide Aq. (10%)
  • Sodium Hydroxide Aq. (50%)
  • Sodium Hypochlorite 15% CI (Chlorine Bleach)
  • Sodium Nitrate Aq. (50%)
  • Sodium Silicate
  • Sodium Sulfate Aq. (90%)
  • Sodium Thiosulfate Aq. (10%)
  • Stannic Sulfate Aq. (10%)
  • Stearic Acid
  • Styrene (Monomer)
  • Sulfur
  • Sulfur Dioxide (Dry Gas) (100%)
  • Sulfuric Acid Aq. (2%)
  • Sulfuric Acid Aq. (5%)
  • Sulfuric Acid Conc.
  • Tallow
  • Tar
  • Tartaric Acid Aq.
  • Tetrachlorethylene
  • Tetrahydrofuran
  • Tetralin
  • Thionyl Chloride
  • Toluene
  • Transformer Oil
  • Trichlorethylene
  • Triethanolamine
  • Trisodium Phosphate Aq. (95%)
  • Turpentine
  • Urea
  • Vaseline
  • Vegetable Oils
  • Vinegar
  • Vinyl Chloride
  • Water
  • Wax (Molten)
  • White Spirit
  • Wines & Spirits
  • Xylene
  • Xylenol
  • Zinc Chloride Aq. (10%)
  • Zinc Oxide
  • Compliance - FDA
  • Machinability
  • Service in Alcohols
  • Service in Aliphatic Hydrocarbons
  • Service in Aromatic Hydrocarbons
  • Service in Chlorinated Solvents
  • Service in Ethers
  • Service in Ketones
  • Service in Strong Acids
  • Service in Strong Alkalies
  • Service in Sunlight
  • Service in Weak Acids
  • Service in Weak Alkalies
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。